OK guys, what's the recommended way to apply TT?  Some of the threads I have read have said to let the coats dry well and truly before the next coat.

Nino - saw this thread (searching on TT) in the forum http://aussiepinball.com/index.php?topic=1256.msg43272#msg43272, and below is an extract of that thread.

"First coat is a light mist
Wait 10 minutes - But not too long or it dries
Second coat is a thick coat, running left to right
Wait 10 minutes
Third coat is a thick coat, running up and down

Leave the glass for at least 24 hours - no more than 48 hours

Third coat is a thin coat - left to right, then immediately up and down

Don't touch for 48 hours - at least !"


From this, it would appear it is not good to let the 1st and 2nd coat of TT dry before applying the subsequent (2nd & 3rd) coat.  Then wait at least 24 hours (but no more than 48), and apply last (thin) coat.